Nhazi na ngbanwe nke ihe nrụnye nke igwe dị fechaa nwere eriri zuru oke
Okwu mmalite nke igwe nkụ (iron) ladle dryers:
The ígwè (iron) ladle dryersna-ejikarị gas ma ọ bụ mmanụ dị ka mmanụ ọkụ na-ekpo ọkụ nchara (iron) ladle, na ọkụ na-adịkarị n'etiti etiti.draya. Igwe ọkụ ahụ nwere akụkụlybelataingikuku, ọkụ ọkụ bụ 800-1000℃, na okpomọkụ naihicha ikeanụ ọhịa bea bụ ihe dịka 1000-1200℃.
Nyocha nke nhazi mbụ nke igwe nkụ (iron) ladle dryer:
Na mbụ, ọ na-anakwere ihe owuwu tiled nke eriri polycrystalline mullite chere na ọkpụrụkpụ mkpuchi nke 250mm. N'ihi na a na-eji igwe nkụ eme ihe n'egbughị oge ma na-ebuli ya ugboro ugboro, ugboro ole mmebi nke ihe owuwu tiled dị oke elu, na-enwekarị ndụ ọrụ nke ọnwa 6-8. Ọ bụ ezie na eriri mullite nwere mmetụta mkpuchi dị mma, n'ihi ọnụ ahịa dị elu ha, ọnụ ahịa nke nrụzi ahụ dị elu, na-eme ka ọrụ na-abawanye ụba, n'iyi nke isi obodo, na mmụba nke ọnụahịa mmepụta.
1. The draya nwere ike iburu okpomọkụ ka 1200 ℃. N'ihi na a na-eji igwe nkụ eme ihe n'oge na-adịghị anya, iji ngwaahịa nwere zirconium dị ka ihe na-eme ka ọ bụrụ ihe mgbagha nwere ike imezu ihe achọrọ ọrụ; Otú ọ dị, nhọrọ nke ngwaahịa polycrystalline na-ebelata okpomọkụ ha na-arụ ọrụ, nke bụ ihe efu kpamkpam.
2. Okpomọkụ nhazi ọkwa nke ngwaahịa nwere zirconium bụ 1400 ° C, na okpomọkụ maka iji ogologo oge eme ihe adịghị ala karịa 1200 ° C. N'iburu n'uche na ebe a na-arụ ọrụ bụ ikuku mbelata akụkụ, ma ọ bụghị maka iji ogologo oge, ngwaahịa nwere zirconium maka iji oge na-eme ihe nwere ike imezu ihe ndị a chọrọ. Ụdị edozi nke CCEWOOL seramiiki eriri modul nwere pickaxe na-arịlịka.
Mgbe emechara usoro ihe mejupụtara tiled nke CCEWOOL seramiiki fiber modul + ceramic fiber blankest, mmetụta mkpuchi thermal nke ihe owuwu ahụ dị mma karịa nhazi mbụ, yana mmetụta nchekwa ike dị ịtụnanya.
Oge nzipu: Mee-10-2021